I-Nickel cobalt manganese oxide (NCM)
Incazelo Yomkhiqizo
Ulwazi Oluyisisekelo.
| Ipharamitha | |
| Ubuningi obuqinile | ≥ 2.00g/cm3 |
| Indawo ethile yobuso | 0.35 ± 0.20m2/g |
| H2O | ≤500ppm |
| D10 | ≥3.00μm |
| D50 | 11.50±2.00μm |
| D2 | ≤28.00μm |
| Lokho | 7.00~7.60wt% |
| Ku- | 30.00±1.00wt% |
| I-Co | 12.20±1.00wt% |
| Mn | 16.70±1.00wt% |
| UFe | ≤80ppm |
| Nge | ≤50ppm |
| I-PH | 10.80-11.70 |
| Izinto zangaphandle ezisebenzisa ugesi (Fe+Cr+Zn) | ≤ 100ppb |
| Umthamo othize uwukuthi | ≥ 153mAh/g“ |
| Ipharamitha | |
| Ubuningi obuqinile | ≥ 1.80g/cm3 |
| Indawo ethile yobuso | ≤ 0.90m2/g |
| H2O | ≤500ppm |
| D10 | ≥2.00μm |
| D50 | 5.00± 1.50μm |
| D90 | ≤15.00μm |
| Lokho | 7.40±0.20wt% |
| Ku- | 36.30±1.00wt% |
| I-Co | 12.60±1.00wt% |
| Mn | 11.30±1.00wt% |
| UFe | ≤50ppm |
| Nge | ≤20ppm |
| Lokho | ≤400ppm |
| Lokho | ≤150ppm |
| I-Mg | ≤150ppm |
| I-PH | 10.80~11.60 |
| Izinto zangaphandle ezisebenzisa ugesi (Fe+Cr+Zn) | ≤ 100ppb |
| Umthamo othize uwukuthi | ≥ 172.0mAh/g |
| Ukusebenza kahle kokuqala | ≥ 86.0%“ |
| Ipharamitha | |
| Ukuminyana okuxegayo | ≥ 1.20g/cm3 |
| Ubuningi obuqinile | ≥ 2.10g/cm3 |
| Indawo ethile yobuso | 0.25 ± 0.15m2/g |
| H2O | ≤400ppm |
| D10 | ≥5.00μm |
| D50 | 13.00±2.00μm |
| D90 | ≤30.00μm |
| Lokho | 7.40±0.20wt% |
| Ku- | 47.50±1.50wt% |
| I-Co | 6.60±0.60wt% |
| Mn | 5.50±0.60wt% |
| UFe | ≤50ppm |
| Nge | ≤50ppm |
| Lokho | ≤500ppm |
| Lokho | ≤200ppm |
| I-Mg | ≤200ppm |
| i-pH | 11.60±0.20 |
| Izinto zangaphandle ezisebenzisa ugesi (Fe+Cr+Zn) | ≤ 50ppb |
| Umthamo othize uwukuthi | ≥ 190.0mAh/g |
| Ukusebenza kahle kokuqala | ≥ 85.0% |
| I-Li+ yamahhala | ≤2700 ppm" |