Nikel kobalt marganes oksidi (NCM)
Önümiň düşündirişi
Esasy maglumatlar.
| Parametr | |
| Gatyk dykyzlyk | ≥ 2.00g/sm3 |
| Ýeriň anyk meýdany | 0,35 ± 0,20m2/g |
| H2O | ≤500ppm |
| D10 | ≥3.00μm |
| D50 | 11.50±2.00μm |
| D2 | ≤28.00μm |
| Şol | 7.00~7.60wt% |
| Içinde | 30.00±1.00wt% |
| Ko | 12.20±1.00wt% |
| Mn | 16.70±1.00wt% |
| Fe | ≤80ppm |
| Bile | ≤50ppm |
| PH | 10.80-11.70 |
| Magnit daş jisim (Fe+Cr+Zn) | ≤ 100ppb |
| Anyk kuwwatlylyk | ≥ 153mAh/g“ |
| Parametr | |
| Gatyk dykyzlyk | ≥ 1.80g/sm3 |
| Ýeriň anyk meýdany | ≤ 0.90m2/g |
| H2O | ≤500ppm |
| D10 | ≥2.00μm |
| D50 | 5.00± 1.50μm |
| D90 | ≤15.00μm |
| Şol | 7.40±0.20wt% |
| Içinde | 36.30±1.00wt% |
| Ko | 12.60±1.00wt% |
| Mn | 11.30±1.00wt% |
| Fe | ≤50ppm |
| Bile | ≤20ppm |
| Şol | ≤400ppm |
| Şol | ≤150ppm |
| Mg | ≤150ppm |
| PH | 10.80~11.60 |
| Magnit daş jisim (Fe+Cr+Zn) | ≤ 100ppb |
| Anyk kuwwatlylyk | ≥ 172.0mAh/g |
| Ilkinji netijelilik | ≥ 86.0% |
| Parametr | |
| Boş dykyzlyk | ≥ 1.20g/sm3 |
| Gatyk dykyzlyk | ≥ 2.10g/sm3 |
| Ýeriň anyk meýdany | 0,25 ± 0,15m2/g |
| H2O | ≤400ppm |
| D10 | ≥5.00μm |
| D50 | 13.00±2.00μm |
| D90 | ≤30.00μm |
| Şol | 7.40±0.20wt% |
| Içinde | 47.50±1.50wt% |
| Ko | 6.60±0.60wt% |
| Mn | 5.50±0.60wt% |
| Fe | ≤50ppm |
| Bile | ≤50ppm |
| Şol | ≤500ppm |
| Şol | ≤200ppm |
| Mg | ≤200ppm |
| pH | 11.60±0.20 |
| Magnit daş jisim (Fe+Cr+Zn) | ≤ 50ppb |
| Anyk kuwwatlylyk | ≥ 190.0mAh/g |
| Ilkinji netijelilik | ≥ 85.0% |
| Mugt Li+ | ≤2700 ppm" |