Nickel cobalt aruminiyamu oxide
Tsananguro yeChigadzirwa
Nickel cobalt aruminiyamu oxide: ne molecular formula LiNiCoAlO₂, musanganiswa wayo unosanganisira nickel, cobalt, uye aruminiyamu; Inowanzo shandiswa se cathode material ye lithium-ion batteries, ine simba rakawanda uye kugadzikana kwakanaka kwekupisa, uye inowanzo sanganiswa ne graphite anodes
Ruzivo Rwekutanga.
Lithium cobalt oxide ine mwero wakakwira
| Paramita | |
| Saizi yezvikamu D10 | ≥ 4um |
| D50 | 10.0±2.0um |
| D100 | ≤30.0um |
| Nzvimbo chaiyo yepamusoro | 0.40 ± 0.15m²/g |
| Kuwanda kwekudengenyeka | ≥ 2.20g/cm |
| Kuwanda kwekusimba | ≥ 3.30g/cm² |
| Kugona | ≥ 205mAh/g |
| Kushanda zvakanaka kekutanga | ≥ 86%“ |